Batu Karang

Filter
OrderBy
SortBy
DownloadIconDownload PNGDownloadIconDownload JPGDownloadIconDownload SVG
rocks
kekuatan compressive
katon
kelas
pangopènan
kekiatan
kapasitas panas tartamtu
Hyaloclastite
Tambah mbandhingaké
180.00 n / mm 2
kurang
batuan beku
liyane
awet
0.84 kj / kg k
Shoshonite
Tambah mbandhingaké
175.00 n / mm 2
kurang
batuan beku
kurang
awet
0.79 kj / kg k
Porphyry
Tambah mbandhingaké
150.00 n / mm 2
kurang
batuan beku
kurang
awet
0.71 kj / kg k
Greywacke
Tambah mbandhingaké
120.00 n / mm 2
kurang
rocks sedimentary
kurang
awet
0.71 kj / kg k
Foidolite
Tambah mbandhingaké
80.00 n / mm 2
kurang
batuan beku
kurang
awet
0.79 kj / kg k
Skarn
Tambah mbandhingaké
70.00 n / mm 2
kurang
rocks metamorphic
kurang
awet
0.92 kj / kg k
Slate
Tambah mbandhingaké
30.00 n / mm 2
kurang
rocks metamorphic
kurang
awet
0.76 kj / kg k
Hornfels
Tambah mbandhingaké
5.80 n / mm 2
kurang
rocks metamorphic
kurang
awet
0.84 kj / kg k